Study of the n-hexane effect in fuel-grade ethanol mixtures in terms of stress corrosion cracking pf API 5L X70 steel
Publicado em 27/08/2021
Referência:
SANTOS, Célia Aparecida Lino dos; PIMENTA, Gutemberg de Souza; PANOSSIAN, Zehbour. Study of the n-hexane effect in fuel-grade ethanol mixtures in terms of stress corrosion cracking pf API 5L X70 steel. In: NACE INTERNATIONAL CONFERENCE, 2018, Phoenix, EUA. Proceedings.. Paper 11311. 13 p.