Investigation of stress corrosion cracking of austenitic, duplex and super duplex stainless under drop evaporation test using seawater
Publicado em 13/09/2021
Referência:
PEREIRA, Henrique Boschetti; PANOSSIAN, Zehbour; BAPTISTA, Ilson Palmieri; AZEVEDO, César Roberto de Farias. Investigation of stress corrosion cracking of austenitic, duplex and super duplex stainless steels under drop evaporation test using synthetic seawater. Materials Research, v.22, n.2, jan., 2019.
Acesso ao artigo no site do Periódico:
http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392019000200220
PEREIRA, Henrique Boschetti; PANOSSIAN, Zehbour; BAPTISTA, Ilson Palmieri; AZEVEDO, César Roberto de Farias. Investigation of stress corrosion cracking of austenitic, duplex and super duplex stainless steels under drop evaporation test using synthetic seawater. Materials Research, v.22, n.2, jan., 2019.